Differential scanning calorimetry study of normal portland cement paste with 30% fly ash replacement and of the separate fly ash and ground granulated blast-furnace slag powders

Wei Sha, G.B. Pereira

    Research output: Contribution to conferencePaper

    Original languageEnglish
    Pages295-309
    Number of pages15
    Publication statusPublished - Jul 2001
    EventSeventh CANMET/ACI International Conference on Fly Ash, Silica Fume, Slag and Natural Pozzolans in Concrete - Chennai (Madras), India