Original language | English |
---|---|
Pages (from-to) | 1487-1489 |
Number of pages | 3 |
Journal | Cement and Concrete Research |
Volume | 29 |
Issue number | 9 |
Publication status | Published - Sep 1999 |
Bibliographical note
Teaching or Research: 15147ASJC Scopus subject areas
- Industrial and Manufacturing Engineering
- Ceramics and Composites